JAIC 1988, Volume 27, Number 1, Article 3 (pp. 38 to 39)
JAIC online
Journal of the American Institute for Conservation
JAIC 1988, Volume 27, Number 1, Article 3 (pp. 38 to 39)

A NOTE ON THE TREATMENT OF TWO GELATIN SILVER PHOTOGRAPHS BY HAROLD EDGERTON FROM THE PORTFOLIO “SEEING THE UNSEEN”

Meredith Mickelson



NOTES

1.. Edgerton, Harold, “Seeing the Unseen,” Colophon, p. 2 of portfolio included in the complete the set, 1977.

2.. Peter Kluge, Hans Neshen Gmbh Co. KG, P.O.B. 1340, D-3062 Buchberg, Federal Republic of Germany

3.. Hopwood, Walter, Report No. 4424, Conservation Analytical Laboratory Smithsonian Institution, Washington D.C. 20560.

4.. Conversation with Hans J. Denstroff Filmolux Inc., Buffalo, N.Y. (1987).