CONTROLLING THE REFRACTIVE INDEX OF EPOXY ADHESIVES WITH ACCEPTABLE YELLOWING AFTER AGING

CHRISTOPHER C. AUGERSON, & JOHN M. MESSINGER


ABSTRACT—Mixtures of Ablebond and HXTAL NYL-1 were found to produce epoxies with a range of refractive indexes from 1.515 to 1.565. Their yellowing after dark aging is measured and determined to be acceptable for glass repair.

Article Sections:

1. INTRODUCTION
2. EXPERIMENTAL
3. RESULTS
4. CONCLUSIONS
a: Notes , References , Author Information
Entire Article

Copyright 1993 American Institute for Conservation of Historic and Artistic Works