ULTRASONIC MISTING. PART 2, TREATMENT APPLICATIONS

CAROLE DIGNARD, ROBYN DOUGLAS, SHERRY GUILD, ANNE MAHEUX, & WANDA McWILLIAMS



3 HEALTH CONSIDERATIONS

Misting, even of aqueous solutions, should be done with the appropriate safety equipment, such as a respirator, extraction system, or a fume hood. The inhalation of small droplets of adhesive or solvent may contribute to serious health problems.