JAIC 2001, Volume 40, Number 1, Article 5 (pp. 59 to 68)
JAIC online
Journal of the American Institute for Conservation
JAIC 2001, Volume 40, Number 1, Article 5 (pp. 59 to 68)

REGALREZ IN FURNITURE CONSERVATION

HANS PIENA




REFERENCES

Carlson,S. M., and A. P.Schniewind.1989. Residual solvents in wood-consolidant composites.Studies in Conservation35:26–32.

Hercules Inc.1998a. Regalrez 1018, 1085, 1094, and 1126 hydrocarbon resins. Product data sheet. January 27. Wilmington, Del.

Hercules Inc.1998b. Regalrez 1128 and 1139 hydrocarbon resins. Product data sheet. January 27. Wilmington, Del.

Hercules Inc.1998c. Regalrez hydrocarbon resin. Product data sheet. January 27. Wilmington, Del.

Horie, C. V.1994. Materials for conservation, organic consolidants, adhesives and coatings. Oxford: Butterworth-Heinemann Ltd.

Landrey, G. J., 1990. The use of fluorescent microscopy in furniture conservation. ICOM Committee for Conservation preprints, 9th Triennial Meeting, Dresden. Paris: ICOM. 2:835–39.

National Gallery of Art, 1996. Synthetic low molecular weight resins: Europe information sheet. October 31. Washington, D.C.

Rie, E. R. de la.1987. The influence of varnishes on the appearance of paintings. Studies in Conservation32:1–13.

Rie, E. R.de la.1993. Polymer additives for synthetic low-molecular-weight varnishes. ICOM Committee for Conservation preprints, 10th Triennial Meeting, Washington, D.C. Paris: ICOM. 2:566–73.

Rie, E. R.de la, and C.W.McGlinchey. 1990. New synthetic resins for picture varnishes. In Cleaning, retouching and coatings,ed.J. S.Mills and P.Smith. London: International Institute for Conservation of Historic and Artistic Works. 168–73.

Schoeler, C. von, and R.Stoian1994. Transparante kunstharzgebundene Retuschen auf historischen Holzoberflächen? Lassen sich Untersuchungen zu synthetischen Gemäldefirnissen auf Probleme der Möbelrestaurierung übertragen und nutzbar machen? Zeitschrift für Kunsttechnologie und Konservierung8(1):150–57.

Shell Chemicals Co.1995. Kraton polymers for coatings. Product data sheet. SC: 1757-93R. July. Houston, Texas.

Smit, R.1999. Personal communication. Hercules Inc., Ryswÿk, the Netherlands.

Whitten,J.1995a. Low-molecular-weight resins for picture varnishes.AIC postprints, American Institute for Conservation 23d Annual Meeting, St. Paul, Minn.Washington D.C.: AIC.124–29.

Whitten,J.1995b. Regalrez 1094: Properties and uses.WAAC Newsletter17:11–12.



SOURCES OF MATERIALS

Regalrez

Hercules Inc. Resin Division 500 Hercules Rd. Wilmington, Del. 19808-1599 www.herc.com/businesses/resins.htm

Kraton G1650, Shellsol TD, Shellsol D40, Shellsol D70

Shell Chemical Co. Houston, Tex. 77251

Tinuvin 292

Ciba-Geigy Additives Division Hawthorne, N.Y. 10532

White spirit

Kwastex B.V. Postbus 219 7600 AE Almelo The Netherlands

n-hexane, xylene

Aristoforma–Interchema Postbus 75560 1118 ZP Schiphol The Netherlands


AUTHOR INFORMATION

HANS PIENA received his M.Sc. in archaeology at the University of Amsterdam (1992) and his B.A. in the conservation of furniture and interiors at the University of Professional Education (1995) in Amsterdam. Pregraduate internships included work in the furniture conservation laboratories at the Rijksmuseum in Amsterdam and the H. F. du Pont Winterthur Museum in Wilmington, Delaware. Piena is currently the head of wood conservation at the Regional Conservation Laboratory of the Province of Gelderland, where he is responsible for the preventive and active conservation of wooden objects of the 130 museums and 75 historical societies in the region and the training of conservation interns and museum personnel. He was recently appointed as senior tutor for the conservation of furniture at the University of Professional Education in Amsterdam. Address: Gelders Oudheidkundig Contact, Postbus 4040, 7200 BA Zutphen, The Netherlands. E-mail: H.Piena@chello.nl